Properties
- Physical Form
- Typical Properties
Value Units Test Method / Conditions Tensile Strength (at Break, MD) 27 MPa ASTM D 882 Tensile Strength (at Break, TD) 20 MPa ASTM D 882 Strain (at Break, MD) 285 % ASTM D 882 Strain (at Break, TD) 590 % ASTM D 882 Elasticity Modulus (Secant 1%, MD) 178 MPa ASTM D 882 Elasticity Modulus (Secant 1%, TD) 180 MPa ASTM D 882 Elmendorf Tear Strength (TD) 250 gF ASTM D 1922 Dart Drop Impact Strength 160 gF ASTM D 1709/A Haze 8 % ASTM D 1003 - Control Properties
Value Units Test Method / Conditions Melt Flow Rate (at 190°C, 2.16kg) 0.8 g/10 min ASTM D 1238 Density 0.923 g/cm³ ASTM D 792 - Note
Film properties were tested with a monolayer 50 μm thickness blown film, blow-up ratio: 2.8, die gap: 1.8 mm. The optimum processing conditions will vary according to the type of equipment used and cannot be considered a performance guarantee.